01A technician has a stone cast of a premolar with a large pointed buccal cusp, a very small nonfunctional lingual cusp, a prominent transverse ridge and a mesiolingual developmental groove. Which tooth is it?
سؤال تدريبي الوحدة: تشريح الأسنان والإطباق
أMandibular first premolar ✓ الإجابة الصحيحة
A dominant buccal cusp, tiny nonfunctional lingual cusp, transverse ridge and mesiolingual groove together identify the mandibular first premolar.
بMandibular second premolar
The mandibular second premolar has a well-developed lingual cusp or cusps and lacks the mesiolingual groove and strong transverse ridge.
جMaxillary first premolar
The maxillary first premolar has two well-developed cusps of similar height and a mesial depression, not a tiny lingual cusp.
دMaxillary second premolar
The maxillary second premolar has two nearly equal cusps and a smooth mesial surface, unlike a very small lingual cusp.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 1 تشريح الأسنان والإطباق، ص 2؛ Woelfel and Scheid, Dental Anatomy: Its Relevance to Dentistry, latest edition
اسأل صديقًا
02Two cast alloys of similar cost are considered for a crown whose thin margin will be burnished against the die. Alloy P has a lower yield strength and greater percent elongation than alloy Q. Which choice and reason are correct?
سؤال تدريبي الوحدة: المواد السنية
أAlloy P, because it deforms plastically at low stress and stretches without cracking ✓ الإجابة الصحيحة
Burnishing is plastic deformation; low yield strength lets the margin adapt with modest force, and high elongation prevents cracking as it is worked.
بAlloy Q, because its higher yield strength lets the margin hold its shape when burnished
High yield strength resists plastic flow, so the margin would resist adaptation and need excessive force, risking distortion of the casting.
جAlloy Q, because its lower elongation means less springback at the margin
Low elongation signals limited ductility, so burnishing could crack the margin; springback depends on the yield-to-modulus ratio, not elongation.
دAlloy P, because a lower yield strength always means a lower modulus of elasticity
Yield strength and modulus are independent; lower yield says nothing about stiffness, so this reason is unsound even though alloy P is the right choice.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 2 المواد السنية، ص 2؛ Anusavice, Phillips' Science of Dental Materials, latest edition
اسأل صديقًا
03Two alginate impressions of the same arch are made. One is left in open air for an hour, the other is stored immersed in water for an hour, then both are poured. What is expected?
سؤال تدريبي الوحدة: التركيبات الكاملة المتحركة
أBoth casts are accurate because the set gel is dimensionally stable
Set alginate exchanges water with its surroundings, so it is not dimensionally stable in air or water.
بThe air-stored cast is undersized and rough; the water-stored cast is enlarged ✓ الإجابة الصحيحة
Syneresis in air shrinks and roughens the gel, while imbibition in water swells it, giving a larger cast.
جThe air-stored cast is enlarged; the water-stored cast is undersized and rough
This reverses the effects; air loses water and shrinks the gel, whereas immersion swells it.
دBoth casts are undersized because the gel contracts as it ages
Immersion would add water, not remove it; only the air-stored impression would contract.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 3 التركيبات الكاملة المتحركة، ص 2؛ Anusavice, Phillips' Science of Dental Materials, latest edition
اسأل صديقًا
04A die poured from a PVS impression of a premolar has no stone detail along a short stretch of the finish line, where the impression held a bubble. What is the best action?
سؤال تدريبي الوحدة: التركيبات الثابتة
أEstimate the missing line from the impression and carve it into the die
Guessing the line places the margin where the technician imagines it, so the crown may be over- or underextended on the tooth.
بFill the void in the die with wax and judge the margin by eye
Wax cannot recreate the true margin, so a pattern judged by eye reproduces a line that may not exist on the tooth.
جReturn the impression and ask the dentist to retake it ✓ الإجابة الصحيحة
The finish line is not recorded there, so the margin cannot be reconstructed and a retake is the only safe choice.
دSmooth over the void with die hardener and use the impression as poured
Hardener only coats the surface and cannot restore finish-line detail that the impression never recorded in the first place.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 4 التركيبات الثابتة، ص 2؛ Rosenstiel, Land and Fujimoto, Contemporary Fixed Prosthodontics, 5th edition
اسأل صديقًا
05A mandibular Class I arch has sound first premolars as principal abutments. The dentist wants to reduce torque on them when the tissue-supported bases move under load. Which retainer assembly is best?
سؤال تدريبي الوحدة: التركيبات الجزئية المتحركة
أDistal rest with a circumferential clasp engaging a distobuccal undercut
A distal rest causes the abutment to tip distally, and a distobuccal retentive arm increases torque when the base rotates.
بMesial rest, proximal plate and I-bar at the buccal gingival third ✓ الإجابة الصحيحة
The mesial rest moves the fulcrum forward, so the I-bar and proximal plate swing gingivally and disengage when the base is loaded.
جMesial rest with a circumferential clasp engaging a mesiobuccal undercut
The mesial rest helps, but a retentive circumferential arm still tightens on the tooth and does not release torque as an I-bar does.
دDistal rest with a bar clasp and no distal proximal plate or guide plane
A distal rest with no proximal plate has no way to release stress and puts the abutment at greatest torque risk.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 5 التركيبات الجزئية المتحركة، ص 2؛ McGivney, Carr and McCracken, McCracken's Removable Partial Prosthodontics, latest edition
اسأل صديقًا
06On a master cast verified as accurate, a cast screw-retained framework is seated and the screw at one terminal abutment is tightened, and a gap appears at the opposite terminal abutment. What does this indicate, and what is the usual next step?
سؤال تدريبي الوحدة: تركيبات الزرعات السنية
أThe fit is acceptable because tightening the other screws closes the gap
Pulling a misfitting framework down with screws creates stress on implants, so this gap cannot be accepted.
بThe framework is not passive, so it is sectioned and rejoined ✓ الإجابة الصحيحة
A gap with a verified cast shows framework distortion, so the framework is sectioned and rejoined with the segments seated.
جThe cast is inaccurate, so a new impression is required
The cast was verified accurate, so the cause lies in the framework, not the impression or cast.
دThe analog is loose, so the cast must be repoured
A loose analog would be found during cast verification, and repouring would not correct framework distortion.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 6 تركيبات الزرعات السنية، ص 2؛ Drago and Peterson, Implant Laboratory Procedures: A Step-by-Step Guide, latest edition
اسأل صديقًا
07A Hawley retainer fits the master cast perfectly, but the patient cannot seat it fully in the mouth when it is delivered three weeks after the impression. Which cause is most consistent?
سؤال تدريبي الوحدة: أجهزة تقويم الأسنان
أPolymerization shrinkage of the baseplate acrylic during processing
Shrinkage of the acrylic would also prevent seating on the master cast, which the retainer fits perfectly, so it is not the cause.
بDistortion of the labial bow during trimming
A distorted bow would also show when the retainer is tried on the master cast, so this cannot explain the finding.
جExpansion of the stone cast while the appliance was processed
Stone expansion would make the appliance slightly larger than the mouth, giving looseness, not a failure to seat, and the cast fit stays good.
دShifting of the teeth in the arch during the laboratory period ✓ الإجابة الصحيحة
Only a change in the mouth explains a fit on the cast but not on the teeth; teeth shift when no appliance holds them.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 7 أجهزة تقويم الأسنان، ص 2؛ Johnson, Patrick, Stokes, Wildgoose and Wood, Basics of Dental Technology: A Step by Step Approach, 2nd edition
اسأل صديقًا
08A lead-lined shielding stent is made for a patient with metal restorations in the beam path. Why must the lead surface facing the tissues be covered with a layer of acrylic?
سؤال تدريبي الوحدة: تركيبات الوجه والفكين
أTo raise attenuation of the primary beam through the lead
Attenuation depends on lead thickness; the acrylic covering adds almost nothing to blocking the primary beam.
بTo protect the lead sheet from heat distortion during acrylic processing
Acrylic processing temperatures do not distort lead sheet, so the tissue-side layer is placed for dose reasons, not heat protection.
جTo stop the lead from corroding in saliva during the course of treatment
Encasing lead does keep it out of saliva, but the required tissue-side thickness is set by absorbing scattered electrons.
دTo absorb secondary electrons from the lead before they reach mucosa ✓ الإجابة الصحيحة
Lead emits low-energy secondary electrons; a low-atomic-number acrylic layer absorbs them before they reach the mucosa.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 8 تركيبات الوجه والفكين، ص 2؛ McKinstry, Fundamentals of Facial Prosthetics, latest edition
اسأل صديقًا
09A technician soaks an alginate impression in disinfectant for far longer than the label allows, then pours it. The cast surface is rough and dimensionally inaccurate. Which explanation fits best?
سؤال تدريبي الوحدة: مكافحة العدوى
أResidual disinfectant raised the stone's setting temperature and expanded it
Disinfectant residue does not raise stone temperature enough to distort a cast, and heat would not roughen the surface.
بProlonged immersion let the gel take up liquid and swell, softening its surface ✓ الإجابة الصحيحة
Alginate is a hydrocolloid, so long immersion causes imbibition, swelling and surface breakdown, giving a rough and inaccurate cast.
جThe alginate lost water by syneresis during the soak and shrank
Syneresis is water loss from a gel left in air; immersed in liquid the gel takes up water instead.
دThe stone was mixed with too little water, raising its setting expansion
A low water-powder ratio changes stone strength and expansion but is unrelated to the soak and does not roughen the surface.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 9 مكافحة العدوى، ص 2؛ Anusavice, Phillips' Science of Dental Materials, latest edition
اسأل صديقًا
10A sandblasting cabinet used for cast alloy frameworks is fully enclosed, yet fine dust escapes around the door seal and settles on the bench during use. The seal is intact and the air supply pressure is normal. Which cause is the most likely?
سؤال تدريبي الوحدة: الصحة والسلامة
أA clogged extraction filter that has cut negative pressure inside the cabinet ✓ الإجابة الصحيحة
Reduced extraction airflow lets cabinet pressure rise, so dust-laden air leaks out through small gaps instead of being drawn to the filter.
بAbrasive particles that are too coarse for the alloy being cleaned in the cabinet
Coarser abrasive tends to produce less airborne fine dust, so coarse particles would not explain dust leaking out at the seal.
جGloves in the cabinet that are slightly too small for the operator
Glove fit affects comfort and control but does not change the airflow balance that keeps dust inside an enclosed cabinet.
دAbrasive that has been recycled many times and broken down into fines
Worn abrasive raises the dust load, but working extraction keeps the cabinet under negative pressure, so dust is drawn inward rather than leaking out.
المرجع: دليل محتوى اختبار فني مختبر الأسنان (الهيئة السعودية للتخصصات الصحية، V1.220901)، القسم 10 الصحة والسلامة، ص 2؛ Johnson, Patrick, Stokes, Wildgoose and Wood, Basics of Dental Technology: A Step by Step Approach, 2nd edition